How to Repair Cracks in an Acrylic Tanning Bed

104 25
    • 1). Position your tanning bed in an upright position, ensuring all power cords are unplugged from the electrical source. This eliminates the risk of electrocution. Make sure that your tanning bed canopy is fully opened, to allow you ample space to work, without risk of injury to you or the bed.

    • 2). Locate the bed profiles that hold your acrylic in place. These are made of pliable materials, and form a hinge over your acrylic, running the entire length of the tanning bed. Pull up at the middle of the open side, to release your acrylic. Some beds contain two sets of profiles for additional stability, therefore you may be required to repeat the release process, on these additional profiles.

    • 3). Grasp your acrylic by the outer edge nearest you. Avoid sharp edges, as they pose a cutting risk. With the outer edge firmly in your hands, carefully slide the acrylic towards you, releasing it from the inner profiles.

    • 4). Set your damaged acrylic against a wall, out of your working space. Firmly grasp your new acrylic by the outer edge, as you did for removal of the old one. Position your new acrylic to line-up perfectly with the inner profiles of your tanning bed -- and carefully slide it into place.

    • 5). Press gently on the new acrylic, around the profiles to secure. You will hear and feel a soft click, letting you know that the acrylic has been positioned properly.

    • 6). Follow installation with a thorough cleaning, using a non-alcohol based cleanser specifically formulated for acrylic surfaces.

Subscribe to our newsletter
Sign up here to get the latest news, updates and special offers delivered directly to your inbox.
You can unsubscribe at any time

Leave A Reply

Your email address will not be published.